Meta description: Tack determines whether stretch film holds a pallet or unwinds in transit. Compare one-sided and two-sided cling, how tack is built in, and why film loses grip.
Stretch film tack is the controlled surface stickiness that bonds film layers to each other on a wrapped pallet. Without it, film of the same thickness and stretch ratio produces a loose load that shifts inside a container. Tack is designed into the film through additives and skin layers, and it changes with age, temperature and handling. Buyers who specify the cling side and the cling level avoid both slipping loads and rolls that block on the unwind.
Table of Contents
- What Is Tack in Stretch Film?
- How Tack Is Built Into the Film
- One-Sided vs Two-Sided Cling
- Why Stretch Film Loses Grip
- Measuring and Specifying Cling
- Common Buying Mistakes
- Specifications to Check in an RFQ
- Frequently Asked Questions
- Source PE Stretch Film from Pefilmpack
What Is Tack in Stretch Film?
Tack is the property that makes two layers of film grip when they touch and release when they are pulled apart. Unlike packing tape, stretch film carries no adhesive coat; the bond is temporary, pressure-sensitive and reversible, produced by the polymer surface plus a small amount of additive that migrates to it.
On a pallet, tack does three jobs. It stops the tail unwinding in transit, it locks each revolution to the one beneath so the wrap behaves as a single sleeve, and it closes the small gaps that open when a load settles. Film with weak tack can pass a containment check on wrapping day and still arrive with a loose top layer after a week at sea.
Tack also carries cost. Higher cling means more additive, a more complex coextruded structure and tighter process control, plus blocking risk: a roll that grips itself too strongly will not unwind cleanly at the start of a new pallet.
How Tack Is Built Into the Film
Base resin supplies strength; tack is added on top of that foundation.
- Resin selection. Linear low-density and metallocene grades set tensile strength, puncture resistance and elongation, and contribute some natural cling — not enough for a heavy pallet.
- Tackifier masterbatch. Polyisobutylene is the standard choice in PE stretch film, with EVA-based systems used where the balance of cling, clarity and cost is different. Dosage is small and must suit the resin and the season.
- Coextrusion. On multilayer lines the tackifier is concentrated in one or two thin skin layers instead of the whole web, which keeps the core strong and the surface active. This is how one-sided cling is made.
- Cooling and winding. Chill roll settings shape the skin, and winding tension decides how hard the layers press on each other in the roll. Wound too tight, a roll blocks even at moderate tack.
- Ageing before shipment. Tackifier needs days to migrate to the surface, and the same migration continues in your warehouse. A roll that is perfect at the plant can be over-tacky or dried out months later.
Cling is therefore a formulation decision, not a thickness decision: two rolls of identical gauge from different plants can behave very differently on the same wrapper. Our comparison of blown versus cast stretch film explains how the process route changes surface behaviour.
One-Sided vs Two-Sided Cling
Cling can sit on the inside face of the roll only, on both faces, or on the outside face only. Each configuration suits a different wrapping method.
| Configuration | Where the tack sits | Behaviour on the pallet | Best suited to |
|---|---|---|---|
| Single-sided, inside cling | Inner surface of the web | Layers bond through the wrap; the outside of the finished pallet stays smooth | Machine wrapping, mixed loads, pallets that must slide past each other in a container |
| Double-sided cling | Both surfaces | Stronger layer-to-layer lock and firmer tail adhesion, with louder unwind | Hand wrapping, light or unstable loads, short wraps that rely on the tail |
| Low-cling or non-cling | Minimal or none | Layers slide rather than bond; containment comes from tension alone | Crush-sensitive goods, and film used as a dust cover over strapped loads |
Selection advice: for automatic and semi-automatic pallet wrapping, single-sided inside cling is usually the practical default, because double-sided film raises drag and noise on a high-speed carriage. Choose double-sided cling for hand wrapping and for light stacks where every layer must grip. Low-cling film belongs where strapping or a shrink hood provides the containment and the film only keeps dust off.
Why Stretch Film Loses Grip
Complaints that film “used to hold” usually trace back to one of these causes.
- Ageing. Tackifier keeps migrating after production. Fresh film may block; long-stored film can dry out and lose grip. Order in cycles that match consumption.
- Heat. A hot container softens the film, increases blocking and distorts the roll. Store away from sunlight and hot walls.
- Cold. Low temperature stiffens the polymer and reduces effective tack. Our guide to cold storage stretch film covers freezer and reefer selection.
- Contamination. Corrugated dust, flour, sand and carton coatings sit between layers and kill the bond. Pallets that are clean and dry hold better than pallets that are not.
- Over-stretching. Past the film’s limit the web thins, the tack skin stretches out and edge tears begin. Additive cannot compensate for a ratio the film was not built for.
- Wrong orientation. A single-sided roll threaded cling-out grips the pallet weakly and the outside of the wrap not at all. Mark the cling side on the core and check direction at every roll change.
- Condensation. Moisture on cartons or film acts as a release layer, so wrapping cold goods in a warm, humid bay is a classic failure.
Measuring and Specifying Cling
Cling is reported as a comparative value. Two plies are pressed together under a controlled roller load, peeled at a fixed angle and speed, and the force is recorded. Because no single international pass limit exists, values are comparable only within the same method. ASTM D4649, the standard guide for selection and use of stretch wrap films, is the usual reference for evaluating properties in application.
When a supplier quotes a cling figure, ask for the test method, the units, whether the value refers to film-to-film or film-to-carton grip, and the storage age of the sample. A number without that context is marketing rather than specification.
In the plant, run a comparative trial: wrap ten representative pallets with the incumbent film and ten with the candidate on the same machine recipe, check the tail after 24 hours, push the top layer sideways by hand, and run a short transport test where practical. Our stretch film quality testing guide sets out the incoming inspection steps.
Common Buying Mistakes
- Buying on gauge alone. A 20 micron film with a weak tack skin can hold less than an 18 micron film with a properly formulated one.
- Switching cling side without telling the machine operator. A roll loaded backwards looks like a quality failure but is an orientation error.
- Comparing price per roll. Cost per pallet wrapped is the number that matters; the cost per pallet calculation shows how to build it.
- Ordering a full year at once. Tack and blocking behaviour drift during storage, so a stock that is comfortable in month one may be unusable in month ten.
- Specifying maximum tack. Film that blocks, tears at the start of a roll or fogs a printed carton costs more than the extra grip saves.
Specifications to Check in an RFQ
Put these points in writing so the quotation and the delivery can be compared line by line:
- Thickness in microns with the tolerance band, and the gauge equivalent if you work in mils
- Width in millimeters, plus roll length or roll weight
- Core inner diameter, commonly 76 mm or 50 mm, and core material
- Cling configuration: single-sided inside, single-sided outside or double-sided
- Target cling level and the test method used to verify it
- Elongation and tensile values with the method applied, such as ASTM D882
- Puncture or dart impact data such as ASTM D5748 where sharp edges are involved
- Hand grade or machine grade, and the pre-stretch ratio the film is designed for
- Colour, transparency and any printing or core marking requirement
- Order quantity, packaging format, destination port and shipping terms
Requirements may vary by application, market and applicable standard. A specification that performs on a 1,200 mm pallet of bagged goods may need revision on an oversized pallet with sharp steel edges; see our guide to stretch film thickness and width for export pallets.
Frequently Asked Questions
Is double-sided cling stronger than single-sided?
For layer-to-layer grip, yes. Double-sided film bonds on both faces, so each revolution locks to the layer above and below. It also raises unwind force and noise, which is why automatic lines normally prefer single-sided inside cling.
Why does my film block and tear at the start of a roll?
Usually excess tack combined with tight winding or warm storage. Ask for a lower cling level, confirm the roll was not stored hot, and check winding tension.
Can tack be measured before shipping?
Yes, but only comparatively. Suppliers run an in-house peel test and report a value with method and units. Ask for the method so you can compare like with like.
Does thicker film always grip better?
No. Thickness adds strength and puncture resistance; grip comes from surface formulation. A thin film with a well-built tack layer can outperform a thick one with a weak layer.
How long can stretch film be stored?
Plan on months rather than years. Keep rolls sealed, out of sunlight and below the temperature where the film softens, and rotate stock so old rolls are used first.
Does cling matter for hand wrapping?
It matters more. Hand wrapping relies on layer grip instead of high machine tension, so double-sided or higher-cling film is normally the better choice.
Source PE Stretch Film from Pefilmpack
Weishan Litong Packing Material Co., Ltd. produces PE stretch film in hand grade and machine grade, with cling level, thickness, width, roll weight, core size and colour agreed to your specification rather than taken from a catalogue. Film is available in single-sided and double-sided cling configurations, and specifications can be matched to your wrapping method, load type and climate.
To receive a quotation, send us the film type, thickness and width, roll weight or roll length, core size, cling requirement, order quantity, packaging preference and destination port. We will reply with a specification sheet and an export quotation, and samples can be supplied for a line trial before you commit to production.