Meta description: A buyer’s guide to silage bunker cover film: barrier layers, thickness and UV grades, weighting and sealing practice, cost per tonne and supplier checks.
A silage bunker cover is the film that seals a compacted pit of forage against oxygen until the face is reopened for feed-out. Buyers specify it by thickness, width, UV grade and layer structure rather than by price per kilogram.
Air reaching stored forage restarts respiration, and dry matter is converted to heat and carbon dioxide within days. The cover is therefore judged on installed cost per tonne of silage, not on price per roll.
Table of Contents
- What Does a Silage Bunker Cover Actually Do?
- How Bunker Cover Film Is Manufactured
- Which Cover Structures Are Available?
- Bunker Cover Film vs Bale Wrap Film
- What Specifications Should Buyers Confirm?
- Weighting and Sealing: Where Most Bunkers Fail
- What Does Cover Film Cost per Tonne of Silage?
- Common Procurement Mistakes
- How to Inspect Cover Film Before Shipment
- What Should an RFQ Include?
- How to Choose a Silage Film Supplier
- Frequently Asked Questions
- Source Silage Bunker Covers from Pefilmpack
What Does a Silage Bunker Cover Actually Do?
The cover is a physical barrier, and it controls only two of the four routes by which air reaches silage: through the sheet itself, and through seams and edges. Side walls, floor and feed-out face are separate barriers that should be specified with it.
A gas-tight sheet installed without proper weighting performs worse than a plain sheet installed with discipline. That is why the installation method belongs in the purchase specification, not only in the farm’s work plan.
How Bunker Cover Film Is Manufactured
Bunker covers are blown polyethylene film, usually three or five coextruded layers.
- Resin and UV masterbatch selection. The blend sets tensile and puncture behaviour; the UV package sets service life. Ask for both in writing.
- Coextrusion. Separate extruders build a reflective skin, a light-blocking layer and, in barrier grades, an oxygen-barrier layer. Layer structure drives cost more than thickness.
- Online gauging. Continuous thickness measurement across the web prevents thin bands that fail first under gravel or tyres.
- Slitting and winding. Sheets are supplied in wide drops, so a 12 m pit is covered in two or three passes rather than a dozen narrow strips.
- Inspection and export packing. Gauge, width, length, UV months and batch number belong on the label and on the delivery documents.
Which Cover Structures Are Available?
Standard UV-stabilised cover film
White, black or white-on-black polyethylene, commonly 100 to 150 micron, cut to pit width. It suits pits emptied within one storage season; confirm the UV period in months against the intended storage duration.
Oxygen barrier film
Some producers coextrude a barrier layer such as EVOH. Cost per square metre is higher, and the case for it is a high-value top layer or a pit that is opened and reclosed. Ask for oxygen transmission with the test method, not the word “barrier”.
White-on-black two-tone film
A reflective white surface with a light-blocking black underside. Common in hot climates, where a plain black sheet overheats the surface layer.
Side-wall film
Thinner sheeting, often 80 to 100 micron, cut to wall height. It protects the shoulder, the zone where punctures and leaks concentrate.
Bunker Cover Film vs Bale Wrap Film
Both are sold as silage film and they are not interchangeable. Bale wrap has no UV package for months of exposure, no width for practical coverage, and no thickness to survive tyre weighting.
| Property | Bunker cover film | Bale wrap film |
|---|---|---|
| Typical thickness | 100 to 150 micron | 25 to 30 micron |
| Typical width | Wide drops matched to pit width | 500 to 750 mm |
| Application | Laid flat, weighted, seams sealed | Stretched 50 to 70 percent on a wrapper |
| Key property | Puncture and UV resistance | Tack, stretch, low oxygen transmission |
| Typical failure | Wind lift, seam leak, shoulder tear | Wrap damage, too few layers |
Choose cover film for compacted pits and bunkers; choose bale wrap for individually sealed bales.
What Specifications Should Buyers Confirm?
- Thickness and tolerance in micron, stated as nominal plus a permitted range.
- Width and length or roll weight, and whether the sheet is flat, gusseted or centre-folded.
- UV stabilisation period in months, matched to storage length and climate.
- Layer structure, including whether a barrier layer is present and what it is.
- Colour: white, black, white-on-black or a custom shade.
- Mechanical data for demanding sites: tensile and elongation (ASTM D882), tear (ASTM D1922), dart impact (ASTM D1709).
- Core diameter and roll weight, since wide heavy rolls are handled manually on most farms.
Requirements may vary by application, market and applicable standard.
Weighting and Sealing: Where Most Bunkers Fail
The sheet is rarely the weak point. Edges, seams and weighted zones are.
- Continuous weighting. Tyres set in a loose grid leave unweighted panels that flutter, pump air and abrade the film.
- Seam overlap. Roughly 150 to 200 mm, folded rather than butted, with tape or adhesive at critical joints.
- Shoulder and wall junction. The cover should run down the wall and be tucked or taped; stopping at the top edge is the most common leak path.
- Front edge. Re-seal the face after every feed-out, or air is drawn under the sheet along its full length.
- Weekly inspection. In the first month, a short walk of the sheet catches wind lift and bird damage while a patch is still enough.
What Does Cover Film Cost per Tonne of Silage?
The following is an illustrative calculation, not a quoted price. Assume a bunker of 500 tonnes, 12 m wide by 40 m long, so about 480 m2 of cover.
- At 150 micron the film weighs about 138 g/m2, so the cover takes about 66 kg.
- Two side-wall sheets of 40 m by 2.5 m at 100 micron add about 18 kg.
- Total film is roughly 84 kg; at an indicative USD 2.10 per kilogram the bill is about USD 176, or USD 0.35 per tonne of silage.
Now the loss side. At 35 percent dry matter the bunker holds about 175 tonnes of dry matter, so a 5 percent loss destroys roughly 8.75 tonnes. At an indicative USD 150 per tonne of dry matter that is about USD 1,300, more than seven times the film cost.
Forage extension services commonly quote avoidable losses of 5 to 15 percent for poorly sealed bunkers. Treat such ranges as indicative, because density, moisture and climate dominate the outcome. The commercial conclusion does not depend on the exact figure.
Common Procurement Mistakes
- Buying on price per kilogram. A 100 micron sheet with a four-month UV package is not comparable to a 150 micron sheet rated for twelve months.
- Ordering bale wrap for a pit. Wrong thickness, wrong width, no UV protection for long exposure.
- Ignoring pit geometry. Narrow sheets multiply seams; oversized sheets waste material and handle badly in wind.
- No thickness tolerance on the purchase order, which allows a nominal 150 micron delivery to arrive materially thinner.
- Skipping the field trial. One pit reveals handling, tear propagation and whether the sheet stays put under the farm’s own weighting method.
How to Inspect Cover Film Before Shipment
At the factory: thickness measured at several points across the width, width and length or roll weight, core diameter, end-face condition, colour consistency between rolls of one order, label accuracy and export packing.
From batch records: tensile and tear results, dart impact, UV masterbatch loading and the declared stabilisation period, and oxygen transmission for barrier grades. Ask for the date and scope of any third-party report; a report covers the sampled batch, not the shipment.
What Should an RFQ Include?
- Product type: standard cover, barrier cover or side-wall film.
- Structure: layer count, colour combination, barrier layer if required.
- Dimensions: thickness, width, length or roll weight.
- UV period in months and the intended storage duration.
- Core diameter and maximum roll weight for handling.
- Quantity in rolls, tonnes or containers, and trial order intention.
- Pit dimensions, weighting method, destination port and shipping terms.
How to Choose a Silage Film Supplier
- Ask what the UV package is. A supplier who cannot describe the stabiliser system is reselling rather than manufacturing.
- Confirm coextrusion capability, and whether a barrier layer can be quoted as a separate option.
- Request gauge records for the production batch, not only a nominal figure.
- Check width flexibility. Pits are not standard, so slitting to the buyer’s width reduces seams and waste.
- Test the sample on a real pit, and verify that export packing survives container handling without edge damage.
Frequently Asked Questions
How thick should a silage bunker cover be?
Most covers are supplied between 100 and 150 micron. Thicker sheet resists puncture and wind damage better; thinner sheet is easier to handle. Match thickness to weighting method and pit size.
How long does bunker cover film last?
Service life is set by the UV package and by exposure. Specify a UV period longer than the storage season, with margin where the sheet stays on the pit through a hot summer.
Can I use bale wrap film to cover a pit?
No. Bale wrap is 25 to 30 micron with high stretch and tack, made for wrapper application. It lacks the width, thickness and UV protection a weighted pit cover needs.
Is black or white cover film better?
White reflects heat and suits hot climates; black blocks light and hides soiling. White-on-black combines both and is usual where surface temperature is a concern.
How much overlap do cover seams need?
Roughly 150 to 200 mm, folded rather than butted, plus tape at critical joints. Weight alone does not seal a seam against wind pumping.
Can cover film be customised?
Yes. Width, thickness, length, roll weight, colour, core size and print are commonly customised. Provide pit dimensions and storage duration so the specification can be matched to the job.
Source Silage Bunker Covers from Pefilmpack
Weishan Litong Packing Material Co., Ltd. produces polyethylene films and industrial packaging materials for export markets, including silage cover film and bale wrap in UV-stabilised grades. Width, thickness, length, roll weight, colour and core size can be produced to the buyer’s specification, with OEM branding and export packing prepared for container shipment.
Request a quote with product type, thickness, width, roll weight, UV period, quantity and destination port. Background: our silage film thickness and UV guide and the bale wrapping and sealing field guide. Product ranges are listed under silage film.